摘要:以再生微粉作为固化剂,采用干掺和湿掺2种不同的掺入方法对青海省海东市的黄土状盐渍土进行固化,通过无侧限抗压强度试验、SEM和XRD测试探究固化盐渍土的力学特性和微观机理。结果表明:再生微粉的掺入使黄土状盐渍土的抗压强度较天然盐渍土的有明显提升,且湿掺法对固化土的强度影响更为明显;再生微粉掺入后生成的水化硅酸钙、水化铝酸钙具有胶结作用,与再生微粉共同填充在土颗粒的孔隙中,使土体密实度和固化土强度增大。
关键词:再生微粉;盐渍土;固化;力学特性;抗压强度
Abstract:The loess-like saline soil in Haidong City, Qinghai Province was cured by using the regenerated micropowder as the curing agent, and methods of dry blending and wet blending. Mechanical properties and microscopic mechanisms of cured saline soils were investigated by unconfined compressive strength test, SEM and XRD. The results show that the compressive strength of loess-like saline soil is significantly improved by the addition of regenerated fine powder compared with that of natural saline soil, and the wet blending method has a more obvious effect on the strength of the solidified soil. The cemented hydrated calcium silicate and hydrated calcium aluminate are filled in the pores of the soil particles together with the regenerated micropowder, which improves the soil compactness and the strength of the solidified soil.
Keywords:regenerated micropowder; saline soil; curing; mechanical property; compressive strength
参考文献(References):
[1]于天佑.细粒硫酸盐渍土盐冻胀特性及其对路基变形的影响研究[D].兰州:兰州交通大学,2020.
[2]牛玺荣,李志农,高江平.盐渍土盐胀特性与机制研究进展[J].土壤通报,2008,39(1):163-168.
[3]魏占元.青海盐渍土对变电工程的危害与治理措施[J].青海电力,2007(增刊1):40-44.
[4]吕擎峰,申贝,王生新,等.水玻璃固化硫酸盐渍土强度特性及固化机制研究[J].岩土力学,2016,37(3):687-693,727.
[5]吕擎峰,贾梦雪,王生新,等.含盐量对固化硫酸盐渍土抗压强度的影响[J].中南大学学报(自然科学版),2018,49(3):718-724.
[6]柴寿喜,杨宝珠,王晓燕,等.含盐量对石灰固化滨海盐渍土力学强度影响试验研究[J].岩土力学,2008(7):1769-1772,1777.
[7]陈康亮,刘长武,杨伟峰,等.基于生石灰和粉煤灰改良硫酸盐渍土的强度特性[J].科学技术与工程,2020,20(26):10888-10893.
[8]刘诚斌,纪洪广,刘娟红,等.矿渣复合胶凝材料固化滨海盐渍土的试验研究[J].建筑材料学报,2015,18(1):82-87.
[9]WILD S,KINUTHIA J M,JONES G I,et al.Effects of partial substitution of lime with ground granulated blast furnace slag (GGBS) on the strength properties of lime-stabilised sulphate-bearing clay soils[J].Engineering Geology,1998,51(1):37-53.
[10]周琦,邓安,韩文峰,等.固化滨海盐渍土耐久性试验研究[J].岩土力学,2007(6):1129-1132.
[11]张莎莎,谢山杰,杨晓华,等.火山灰改良粗粒硫酸盐渍土路基填料及其作用机理研究[J].岩土工程学报,2019,41(3):588-594.
[12]KANIRAJ S R,HAVANAGI V G.Behavior of cement-stabilized fiber-reinforced fly ash-soil mixtures[J].Journal of Geotechnical and Geoenvironmental Engineering,2001,127(7):574-584.
[13]KANIRAJ S R,HAVANAGI V G.Compressive strength of cement stabilized fly ash-soil mixtures[J].Cement and Concrete Research,1999,29(5):673-677.
[14]ATIS C D,OZCAN F,KILIC A,et al.Influence of dry and wet curing conditions on compressive strength of silica fume concrete[J].Building and Environment,2005,40(12):1678-1683.
[15]刘音,路畅,张浩强,等.建筑垃圾再生微粉胶凝性的实验研究[J].中国粉体技术,2015,21(5):33-36.
[16]马郁.掺建筑垃圾再生微粉混凝土性能试验研究[J].混凝土与水泥制品,2016(10):88-90.
[17]王一名,常立君,李滢.废弃混凝土再生微粉固化盐渍土的强度特性及微观机理研究[J].材料导报,2021,35(增刊2):268-274.
[18]BIN-SHAFIQUE S,RAHMAN K,YAYKIRAN M,et al.The long-term performance of two fly ash stabilized fine-grained soil subbases[J].Resources,Conservation and Recycling,2010,54(10):666-672.
[19]任振东.石灰-粉煤灰固化黄土状硫酸盐渍土的力学及电化学特性的试验研究[D].太原:太原理工大学,2020.
[20]SINGH S,ASWATH M U,RANGANATH R V.Effect of mechanical activation of red mud on the strength of geopolymer binder[J].Construction and Building Materials,2018,177:91-101.
[21]施惠生,夏明,郭晓潞.粉煤灰基地聚合物反应机理及各组分作用的研究进展[J].硅酸盐学报,2013,41(7):972-980.